Supplier & stockist · Hastelloy
Hastelloy C276 — Supplier & Stockist in Mumbai
Hastelloy C276 (UNS N10276) to ASTM B575 from Ramani Steel House, supplier and stockist in Mumbai since 1974. Request current sizes, stock and pricing.
Hastelloy C276 is a nickel-molybdenum-chromium alloy, UNS N10276 / Werkstoff 2.4819. It is supplied to ASTM B575 in round bar, plate and sheet. The standard sets a minimum tensile strength of 689 MPa and a minimum yield strength of 283 MPa in the solution annealed condition. Ramani Steel House supplies it from Mumbai, India — from stock and against order, cut to size, with the mill test certificate for the heat supplied.
Page last updated .
A nickel-molybdenum-chromium alloy with tungsten, and one of the most versatile corrosion-resistant alloys available. Its very low carbon and silicon limits minimise grain-boundary precipitation during welding, so it can be used in the as-welded condition.


Hastelloy C276 supply information
| Grade | C276 |
|---|---|
| UNS designation | N10276 |
| Standards | ASTM B575ASME SB-575ASTM B574ASME SB-574 |
| Material family | Hastelloy |
| Forms | Round Bar · Plate · Sheet · Strip · Rod |
| Processing | Stamping · Punching · Laser Cutting · Waterjet Cutting · Slitting · Shearing · Band Saw Cutting |
| Traceability | Mill test certificate with every order · AS9120:2018 certified |
| Supplied as | Supplier · Stockist · Stockholder · Distributor · Importer · Exporter — Mumbai, India |
| Availability | Ex-stock and against order — confirmed on enquiry |
| Cut to size | Stamping · Punching · Laser Cutting · Waterjet Cutting — no minimum length |
The specification tables below give the limits and minimums set by the standard. The chemistry and properties of the actual heat supplied are reported on its mill test certificate.
Also specified as
- Hastelloy C276 Round Bar
- Hastelloy C276 Plate
- Hastelloy C276 Sheet
- UNS N10276
- Werkstoff 2.4819
- ASTM B575
- ASME SB-575
- ASTM B574
- ASME SB-574
The same material under the names and designations buyers order it by. Quote any one of them and we will supply against it.
Hastelloy C276 equivalent grades
| Grade | C276 |
|---|---|
| UNS | N10276 |
| Werkstoff Nr. (DIN) | 2.4819 |
| Alloy type | Nickel-molybdenum-chromium alloy |
| Specification | ASTM B575 / B574 |
| Density | 8.89 g/cm³ |
Hastelloy C276 chemical composition
| Element | Limit (wt %) |
|---|---|
| Molybdenum (Mo) | 15.0 – 17.0 |
| Chromium (Cr) | 14.5 – 16.5 |
| Iron (Fe) | 4.0 – 7.0 |
| Tungsten (W) | 3.0 – 4.5 |
| Cobalt (Co) | 2.5 |
| Manganese (Mn) | 1.0 |
| Vanadium (V) | 0.35 |
| Silicon (Si) | 0.08 |
| Carbon (C) | 0.010 |
| Phosphorus (P) | 0.04 |
| Sulphur (S) | 0.03 |
| Nickel (Ni) | Balance |
ASTM B575 / B574 limits. Maximum unless a range or a minimum is shown. Actual heat chemistry is reported on the mill test certificate.
Hastelloy C276 mechanical properties
| Property | Minimum — solution annealed |
|---|---|
| Tensile strength | 689 MPa (100 ksi) |
| Yield strength (0.2% offset) | 283 MPa (41 ksi) |
| Elongation | 40 % |
Minimum values required by ASTM B575 / B574 in the stated condition. Tested values for the heat supplied appear on the mill test certificate.
Hastelloy C276 weight chart
Theoretical weight from the nominal density of 8.89 g/cm³. Useful for freight and costing estimates; it is not a stock list, and actual weight varies within dimensional tolerance.
| Thickness (mm) | kg / m² |
|---|---|
| 0.5 | 4.45 |
| 1 | 8.89 |
| 1.5 | 13.34 |
| 2 | 17.78 |
| 3 | 26.67 |
| 4 | 35.56 |
| 5 | 44.45 |
| 6 | 53.34 |
| 8 | 71.12 |
| 10 | 88.90 |
| 12 | 106.68 |
| 16 | 142.24 |
| 20 | 177.80 |
| 25 | 222.25 |
| Bar diameter (mm) | kg / metre |
|---|---|
| 6 | 0.251 |
| 8 | 0.447 |
| 10 | 0.698 |
| 12 | 1.01 |
| 16 | 1.79 |
| 20 | 2.79 |
| 25 | 4.36 |
| 30 | 6.28 |
| 40 | 11.17 |
| 50 | 17.46 |
| 60 | 25.14 |
| 80 | 44.69 |
| 100 | 69.82 |
Hastelloy C276 bar surface finishes
Round bar is quoted by finish as well as by diameter, and the finish changes both the surface and how closely the diameter is held. These are the standard designations — tell us which you need and we will confirm what is available in this grade and size.
| Code | Finish | How it is produced | What you get |
|---|---|---|---|
| HF | Hot finished | Hot rolled or forged, then straightened. | Dark, scaled surface with the widest diameter tolerance. The usual choice where the bar will be machined all over. |
| HRAP | Hot rolled, annealed and pickled | Hot finished, then annealed and pickled to remove mill scale. | Clean matt grey surface with the scale chemically removed, so corrosion resistance is restored. Tolerance as hot finished. |
| ST | Smooth turned (peeled) | Hot finished bar turned or peeled all over on a machine. | Bright machined surface, decarburised and scaled layer removed, closer and more consistent diameter than hot finished. |
| PR | Peeled and reeled | Peeled, then reeled (roller straightened and burnished). | Peeled surface improved by reeling, with better straightness — specified where the bar feeds automatic machines. |
| CD | Cold drawn | Drawn cold through a die. | Bright surface, close diameter tolerance, and higher strength and hardness from the cold work. Common on smaller diameters. |
| BD | Bright drawn | Cold drawn, sometimes with a further light draw or polish. | The brightest of the drawn finishes. Used where the bar's surface is the finished surface. |
| CG | Centreless ground | Turned or drawn, then ground between centreless wheels. | The closest diameter tolerance and best roundness of the standard finishes. Specified for shafts, pins and anything running in a bearing or seal. |
| PL | Polished | Ground, then polished. | Lowest surface roughness, for sealing faces, hygienic service and visible parts. |
Hastelloy C276 applications
- Chemical processing
- Reactors and heat exchangers in reducing and mixed acids.
- Pollution control
- Flue gas desulphurisation scrubbers.
- Pulp & paper
- Bleach plant equipment.
- Pharmaceutical
- Process equipment handling aggressive chemistries.
Industries that specify Hastelloy C276
- Oil & Gas Alloys
Severe sour, chloride and acid conditions beyond the limits of lower alloys.
- Chemical Process Alloys
Reactors and heat exchangers in reducing and mixed acids.
- Pharmaceutical Stainless & Alloys
Process equipment handling reducing acids.
Hastelloy C276 inspection & test certificates
AS9120:2018
The aerospace standard written specifically for stockist distributors. It covers traceability, counterfeit-part prevention and records retention — the controls an aerospace buyer audits before approving a supplier.
Download certificate (PDF)ISO 9001:2015
The general quality management standard, covering how orders, inspection and non-conformances are controlled.
Download certificate (PDF)
Material is supplied with its mill test certificate, reporting the chemistry and mechanical properties of the heat you receive — which is what the limits in the tables above are checked against. If your order needs third-party inspection, additional testing or a specific certificate type, say so with the enquiry and we will confirm what we can arrange before you order.
Hastelloy C276 — frequently asked
- Should I choose Hastelloy C276 or C22?
- C22 carries more chromium, giving better resistance in oxidising media and to localised corrosion in oxidising chlorides. C276 carries more molybdenum, giving better resistance in reducing acids. The choice turns on whether the process is oxidising or reducing — and many are mixed, so send us the full chemistry.
- Can Hastelloy C276 be used as-welded?
- Yes. Its low carbon and silicon limits keep carbide precipitation in the heat-affected zone low enough for most services without post-weld heat treatment. The matching filler metal is ERNiCrMo-4.
Know your exact specification?
Send the grade, form, dimensions and quantity and we will quote against it directly.
Send a detailed enquiry →